水溶性及分散性之氧化鐵奈米粒子之製造方法及其應用
國立成功大學
2004/05/21
具良好水溶性,分散均勻,粒徑6.2 正負 2.2 nm的四氧化三鐵奈米粒 子可藉由兩階段式保護劑的添加以化學共沉澱法成功地製備出來。首 先,先利用保護劑與反應物共存的技術製備出四氧化三鐵奈米粒子, 再加入適量的保護劑達到表面覆蓋完全的目的。形成的水溶性高的四 氧化三鐵奈米粒子並可輕易地與蛋白質及核糖核酸等生物分子結合。 同時,此新型氧化鐵奈米粒子可發展為具高效能的獨立及複合型核磁 共振造影顯影劑。 The well-dispersed and water-soluble Fe3O4 nanoparticles are successfully prepared via two stages of the preparation procedures: first, using the chemical coprecipitation synthesizes Fe3O4 nanoparticles; second, the additional capping agents facilitate the formation of the Fe3O4 nanoparticles with diameter of 6.2 ± 2.2 nm. These aqueous nanoparticles can be readily incorporated with biomolecules such as nucleic acid or protein. The prepared Fe3O4 have also demonstrated distinct T1 and T2 features suitable for the development of functional Magnetic resonance imaging (MRI) contrast agent either by the particle alone or combined with biomolecules for specific targeting.
本部(收文號1060000114)同意該校105年12月30日成大研總字第1054501055號函申請終止維護專利 多填I 係為了系統規則
企業關係與技轉中心
06-2360524
版權所有 © 國家科學及技術委員會 National Science and Technology Council All Rights Reserved.
建議使用IE 11或以上版本瀏覽器,最佳瀏覽解析度為1024x768以上|政府網站資料開放宣告
主辦單位:國家科學及技術委員會 執行單位:台灣經濟研究院 網站維護:台灣經濟研究院